BASE-LOK® FASTENERS
Product Testing Results

Test Report: 101-97
Product: Base-Lok®
Test: Rupture Value
Procedure: Dade County Protocol PA 117(B)

Manufacturer
Base Sheet Type
Rupture in (lbf)
Celotex
Hydrostop
215.6
GAF
GAFGLAS #75
174.8
GAF
GAFGLAS Stratavent
218.0
GS Roofing
All Weather / Empire
159.1
GS Roofing
GS Glassbase
191.9
GS Roofing
GS Flex-I-Glas Base
213.3
GS Roofing
PolySMS Base
229.9
Malarkey
#515 Fiberglass Standard Base
187.2
Malarkey
#501 Premium I Modified Base
192.3
Malarkey
#603 Superbase
215.1
Malarkey
#605 Panoply
218.0
Schuller
Glasbase Plus
199.1
Schuller
Ventsulation
208.2
Schuller
Dynabase
209.9
Schuller
Glasbase
180.9
SOPREMA
Sopraglass 100
170.0
SOPREMA
Sopra-G
198.6
SOPREMA
Modified Sopra-G
198.7
SOPREMA
Sopravent
220.0
SOPREMA
Sopralene 180
259.2
U.S. Intec
Intec Bondable Base
161.7
U.S. Intec
Permavent
167.4
U.S. Intec
Intec Ultrabase
171.3
U.S. Intec
1ntec Flex Base 30
207.7
U.S. Intec
Intec P190
241.5

Apply suitable factor of safety to arrive at design loads. The above results were obtained under laboratory conditions.

 

Test Report: 102-97
Product: Base-Lok®
Test: Withdrawal Resistance
Procedure: Dade County Protocol PA 117(B)

Withdrawal Resistance Test Data
Deck Type
Resistance At
3 Days (lbf)
Resistance At 28 Days (lbf)
Static
Withdrawal
Static Withdrawal
Pulsating Withdrawal
200 psi cellular LWC
96.6
181.6
126.5
300 psi cellular LWC
-
186.0
-
180 psi
aggregate LWC
58.0
180.0
142.2
Tectum
-
191.5
-
LWC = Lightweight Concrete Apply suitable factor of safety to arrive at design loads. The above results were obtained under laboratory conditions.